Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CALIBRE™ MEGARAD™ 2081-15 - PC - Trinseo

Material Data Center offers the following functions for CALIBRE™ MEGARAD™ 2081-15:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Calibre Megarad datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 흐름성, MFI 15 g/10min ISO 1133
온도 300 °C -
负荷 1.2 kg -
성형 수축률, 평행 0.6 % ISO 294-4, 2577
ASTM 데이터
용융 흐름성, MFI 15 g/10min ASTM D 1238
온도 300 °C -
하중 1.2 kg -
성형 수축률, 평행 0.006 mm/mm ASTM D 955
기계적 특성단위시험규격
ISO 데이터
인장탄성률 2300 MPa ISO 527
항복강도 62 MPa ISO 527
항복변형률 6 % ISO 527
파단시 강도 68 MPa ISO 527
파단시 신율 130 % ISO 527
굴곡 계수, 23°C 2400 MPa ISO 178
굴곡 강도 97 MPa ISO 178
챠피 노치드 충격 강도, +23°C 25 kJ/m² ISO 179/1eA
아이조드 충격은 노치, +23°C 75 kJ/m² ISO 180/1A
ASTM 데이터
인장탄성률 2206 MPa ASTM D 638
항복강도 62.1 MPa ASTM D 638
파단시 강도 68.3 MPa ASTM D 638
항복변형률 6 % ASTM D 638
파단시 신율 130 % ASTM D 638
굴곡 계수 2413 MPa ASTM D 790
굴곡 강도 96.5 MPa ASTM D 790
로크웰 경도 R 118 - ASTM D 785
아이조드 충격은 노치, 1/8 in 747 J/m ASTM D 256
열적 특성단위시험규격
ISO 데이터
하중하에서의 변형온도, 1.80 MPa 120 °C ISO 75-1/-2
비카트 연화 온도, B 138 °C ISO 306
ASTM 데이터
열팽창 계수, 평행 68.4 E-6/K ASTM D 696
DTUL @ 66 psi 139[ann.] °C ASTM D 648
DTUL @ 264 psi 122 °C ASTM D 648
비카트 연화 온도 143 °C ASTM D 1525
ann.: annealed
전기적 특성단위시험규격
ISO 데이터
전기 압력 17 kV/mm IEC 60243-1
ASTM 데이터
전기 압력, 단기간의 16.5 kV/mm ASTM D 149
소산 인자, 1 MHz 0.002 - ASTM D 150
상대 유전율, 60 Hz 3 - ASTM D 150
상대 유전율, 1 MHz 3 - ASTM D 150
부피 저항 2E17 Ohm*cm ASTM D 257
광학 특성단위시험규격
ASTM 데이터
탁도 2 % ASTM D 1003
광선 투겠淅 85 % ASTM D 1003
굴절 지수 1.59 - ASTM D 542
기타 특성단위시험규격
물에서의 흡수성 0.12 % ISO 62와 유사
조건에서의 흡습성 0.15 % ISO 62와 유사
밀도 1200 kg/m³ ISO 1183
물에서의 흡수성, 24hr 0.15 % ASTM D 570
밀도 1200 kg/m³ ASTM D 792
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 120 °C -
Pre-drying - Time 4 h -
용융수지온도 275 - 295 °C -
성형온도 70 - 90 °C -
도표
점도-변형률 , CALIBRE™ MEGARAD™ 2081-15, PC, Trinseo
전단-변형률 , CALIBRE™ MEGARAD™ 2081-15, PC, Trinseo
비용적-온도(pvT) , CALIBRE™ MEGARAD™ 2081-15, PC, Trinseo
특징
생산 공정
사출 성형
부가물
이형제
특별 특성
투명도, 멸균, Gamma irradiation sterilization, Electron beam (e-beam) sterilization
내화학성에
Radiation Resistance
Certifications
Medical Grade, Biocompatibility ISO 10993
응용
의료
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쨀짼쨘횓 쨔횞 횁횩쩐횙 쩐횈쨍횧쨍짰횆짬, 쨉쩔쩐챌 쨔횞 쩐횈횉횁쨍짰횆짬 짹횢쩔짧
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.